Page 1: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Welding Defects and Discontinuities

Page 2: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

What does weld defect mean?

• Any flaw that compromises the usefulness of a weldment (weld)

Page 3: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

What does weld discontinuity mean?

• An interruption of the typical structure of a material. A discontinuity is not necessarily a defect.

Page 4: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Weld Joint Discontinuities• Inclusions

– Slag

– Wagontracks

– Tungsten

• Spatter

• Arc Craters

• Cracks– Longitudinal

– Transverse

– Crater

– Throat

– Toe

– Root

– Underbead and Heat-affected zone

– Hot

– Cold or delayed

• Misalignment (hi-lo)

• Undercut

• Underfill

• Concavity or Convexity

• Excessive reinforcement

• Improper reinforcement

• Insufficient Fill

• Overlap

• Burn-through

• Incomplete or Insufficient Penetration

• Incomplete Fusion

• Surface irregularity– Overlap

• Arc Strikes

• Base Metal Discontinuities

– Lamellar tearing

– Laminations and Delaminations

– Laps and Seams

• Porosity– Uniformly Scattered

– Cluster

– Linear

– Piping

• Hammer Marks • Heat-affected zone

microstructure alteration• Base Plate laminations• Size or dimensions

Page 5: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Weld Joint Discontinuities• Inclusions

– Slag

– Wagontracks

– Tungsten

• Spatter

• Arc Craters

• Cracks– Longitudinal

– Transverse

– Crater

– Throat

– Toe

– Root

– Underbead and Heat-affected zone

– Hot

– Cold or delayed

• Misalignment (hi-lo)

• Undercut

• Underfill

• Concavity or Convexity

• Excessive reinforcement

• Improper reinforcement

• Insufficient Fill

• Overlap

• Burn-through

• Incomplete or Insufficient Penetration

• Incomplete Fusion

• Surface irregularity– Overlap

• Arc Strikes

• Base Metal Discontinuities

– Lamellar tearing

– Laminations and Delaminations

– Laps and Seams

• Porosity– Uniformly Scattered

– Cluster

– Linear

– Piping

• Hammer Marks • Heat-affected zone

microstructure alteration• Base Plate laminations• Size or dimensions

Page 6: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Misalignment (hi-lo)

• Definition: Joint is out of alignment at the root• Cause: Carelessness

Page 7: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Undercut• Definition: A groove cut at the toe of the weld

and left unfilled.

• Cause: High amperage, electrode angle, long arc length, or rust

Page 8: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Insufficient Fill

• Definition: The weld surface is below the adjacent surfaces of the base metal

• Cause: Improper welding techniques

Page 9: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Burn-through

• Definition: When a hole has been completely melted through the base metal.

• Cause: Excessive heat input.

Page 10: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Incomplete or Insufficient Penetration

• Definition: When the weld metal does not extend to the required depth into the joint root

• Cause: Low amperage, low preheat, tight root opening, fast travel speed, short arc length.

Page 11: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Arc Strike

• Definition: A localized coalescence outside the weld zone.

• Cause: Carelessness

Page 12: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Slag Inclusion

• Definition: Slag entrapped within the weld

• Cause: Low amperage, improper technique, Trying to weld in an area that is too tight.

Page 13: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Spatter

• Definition: Small particles of weld metal expelled from the welding operation which adhere to the base metal surface.

• Cause: Long arc length, severe electrode angles, high amperages.

Page 14: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Cracks• When the metal cracks due to shrinkage,

temperate change, and stress on the weld

Page 15: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Porosity

• Weld metal contamination in the form of a trapped gas being trapped in the molten metal

Page 16: Welding Defects and Discontinuities. What does weld defect mean? Any flaw that compromises the usefulness of a weldment (weld)

Hammer Marks

• When you chip the slag to hard and it dents the weld