seoulnikko€¦ · company name seoul nikko co., ltd business fields welding materials welding...
TRANSCRIPT
![Page 1: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/1.jpg)
www.laspedia.com SeoulNikko
![Page 2: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/2.jpg)
1. Company Overview
Content
2. Organization structure
4. Partners
5. Business
6. Products Line_up
3. Corporate Vision
7. Why PT. Seoul Nikko Indonesia?
![Page 3: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/3.jpg)
1. Company Overview
KOREA
Company Name Seoul Nikko Co., Ltd
Business FieldsWelding MaterialsWelding MachinesWelding Consumables
Establishment 1995. 7
Address Seoul, Korea
Contact +82 2 2611 8558
Project
Experience
IHI, HITACHI, TOSHIBASAMSUNG Heavy Industry FPSOHYUNDAI Heavy Industry FPSO, LNGTank Vessel Project(PETRONAS)DAEWOO Heavy Industry.,etc
INDONESIA
PT.Seoul Nikko Indonesia
Welding MaterialsWelding Consumables
2014. 8
Jakarta, INDONESIA
+62 21 2607 1148
Pertamina Group Refinery Unit KRAKATAU POSCO, Sinar Mas Group Asia Pulp & Paper ,Truba Group, PT. MEIWA Mold,PT. DAIHO, PT.NARA SUMMIT etc.,
![Page 4: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/4.jpg)
2. Organization Structure
C E O
Administration
Division
HRD
&
Accounting
Team
Marketing
Division
Welding
Materials
Team
Welding
ConsumAbles
Team
Technical Suppot
Division
R&D
New Item
Development
Team
Agent
Support
Team
Legal
Support
Team
Board
Of
Director
![Page 5: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/5.jpg)
3. Corporate Vision
The Ultimate Welding Consumables Supplier
Diversity
Customer
Satisfaction
Price
Delivery
Quality
![Page 6: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/6.jpg)
4. Partners
NICHIA
Strategic partnership Sole Distributor Distributor
KOREA
Distributor Distributor Sole Distributor Sole Distributor
Others
Distributor Distributor Distributor Distributor
Taiwan USA USA EU
JAPAN
![Page 7: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/7.jpg)
5. Business fields
Energy & Power Plants
Petro chemical plants, LNG Storage Tank, Power Plants
Offshore Structure
Offshore platform-LNG Vessels, FPSO
Shipbuilding
LPG Tankers, Container vessels
Pipe Industry
Pipe-line installation
Heavy equipment
Repair & maintenanceMining & other equipment, Casting RollsSteel Fabrication
High tensile steel structure
NICHIA
![Page 8: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/8.jpg)
6. Product Line up
Spec (AWS) Welding Process Size Application
E6013
E7016
SMAW 2.0 ~ 5.0 ø
Welding of structures, building, high pressure vessels and step building.
Mild steel and 490MPa Class high tensile strength steel.
* Shielding Gas
GMAW : CO2 or 80% Ar +20% CO2
GTAW : Ar
FCAW : CO2
ER70S-6
ER70S-G
GMAW 0.8 ~ 1.6 ø
ER70S-6
ER70S-G
GTAW 1.0 ~ 3.2 ø
E71T-1C FCAW 1.2 ~ 1.6 ø
F7A(p)6-EH14
F7A4-EL8
F7AZ-E714
SAW
(Submerged-Arc Wel
ding )
2.4 ~ 6.4 ø
MILD STEEL & HIGH TENSILE STRENGTH STEEL
HYUNDAI S-6013LF KISWEL KC-28 (ER70S-6) HYUNDAI SM-70
![Page 9: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/9.jpg)
6. Product Line up
Steel Type SMAW GTAW GMAW SAW
1~1.25Cr – 0,5Mo
1~1.25Cr – 0.5Mo
CM-A96
CM-A96MB(AC)
TG-S1CM
TG-S80B2
MG-S1CM PF-200/US-511N (AC)
PF-200D/US-511ND (DC)
2.25Cr – 1Mo CM-A106 TG-S2CM
TG-S90B3
MG-S2CM PF-200/US-521S (AC)
5Cr – 0,5Mo CM-5 TG-S5CM MG-S5CM PF-200S/US-502 (AC)
9Cr – 1Mo CM-9 TG-S9CM MG-S9CM
9Cr – 1Mo – V - Nb CM-9Cb
CM-96B9
TG-S9Cb
TG-S90B9
MG-S9Cb PF-200S/US-9Cb(AC)
PF-90B9/US-90B9(DC)
9Cr – W – V – Nb
12Cr – W – V - Nb
CR-12S TG-S12CRS MG-S12CRS PF-200S/US-12CRSD(DC)
For Heat-Resistant Steel.
For Heat – Resistant Steel
TG-S1N, TG-S3N
MG-S1N, MG-S3N
For Low Temperature Steel
G-50, G-60, G-80, MF-38, PF-S1 Flux for SAW
TG-X308L, TG-X309L, TG-X316L For One Side Tig Welding
KOBE Steel’s Other Products
Underwater WeldingProduct Name Application
NICHIA AW-01 Underwater welding electrodes for general Mild Steel.
Available all position of welding & keep stable Arc.
NICHIA AW-03 Underwater welding electrodes for 18Cr-8Ni Stainless Steel.
Joint welding of SUS304, SUS + Mild Steel.
NICHIA
![Page 10: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/10.jpg)
6. Product Line up
Spec (AWS) Size (ø) Application
E308-16 1.6, 2.0, 2.6,
3.2, 4.0, 5.0 mm
For Stainless Steel [18%Cr – 8%Ni] 304, 301 and 302.
E308L-16 For Low Carbon Stainless Steel, 304L.
E308H-16
2.6 mm
3.2 mm
4.0 mm
5.0 mm
308H is superior in mechanical properties at high temperature.
E309-16
E309L-16
For 22%Cr – 12%Ni Stainless Steel, Joining of SUS to Steels.
Low Carbon 22%Cr – 12%Ni Stainless Steel.
E309Mo
E309MoL-16
For 22%Cr – 12%Ni – 2.5%Mo Stainless Steel.
Joining of SUS 316 to Ferritic Steel.
E310-16 For 25%Cr – 20%Ni Stainless Steel. SUS310S.
E316-16 For 18%Cr – 12%Ni – 2.5%Mo Stainless Steel. SUS316.
E316L-16 For low carbon 18%Cr – 12%Ni – 2.5% Mo Stainless Steel. SUS316L.
E347-16 For 18%Cr – 8%Ni – Nb or Ti Stainless Steel. SUS347, SUS321.
E410-16 For 13%Cr Stainless Steel. SUS410, SUS420.
E430-16 For 18%Cr Stainless Steel. SUS430, SUS405.
E312-16 For joining of Dissimilar Metal.
STAINLESS STEEL ELECTRODE (SMAW)
Product Name Spec (AWS) Product Name Spec (AWS) Produk Name Spec (AWS)
NS-309HC For SCH13 NS-309Mn For YUS170 NS-310HC For HK40, SCH22
NS-20CbL E320LR-16 NS-2209 E2209-16 NS-329W For SUS-329J4L
NS-2594CW E2594-16 NS-410NiMo E410NiMo-16 NS-630 E630-16
SPECIAL STAINLESS STEEL ELECTRODES (SMAW)
Spec (AWS) GTAW MIG & SAW Spec (AWS) GTAW MIG & SAW
ER308
ER308L
ER309
ER309L
ER309MoL
ER310
ER316
ER316L
ER317L
ER347
ER347L
ER347H
NS-308R
NS-308LR
NS-309R
NS-309LR
NS-309MoLR
NS-310R
NS-316R
NS-316LR
NS-317LR
NS-347R
NS-347LR
NS-347HR
NS-308M
NS-308LM
NS-309M
NS-309LM
NS-309MoLM
NS-310M
NS-316M
NS-316LM
NS-317LM
NS-347M
NS-347LM
NS-347HM
ER410
ER430
ER385
ER320LR
ER410NiMo
ER630
ER2209
ER2594
NS-410R
NS-430R
NS-385R
NS-320LR
NS-410NiMoR
NS-630R
NS-2209R
NS-2594NLR
NS-410M
NS-430M
NS-385M
NS-320LM
NS-410NiMoM
NS-630M
NS-2209M
NS-2594NLM
STAINLESS STEEL TIG – MIG & SUBMERGED ARC WELDING WIRE (SAW)
S-308L.16N
Welding for Stainless Pipe
Welding for Duplex Stainless SteelNS-2209
![Page 11: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/11.jpg)
6. Product Line up
Product Name Welding Process Spec (AWS) Size (ø) Applications
DM-100
DMA-100
DM-150
SDM-31
SMAW
ENi-CI
ENiFe-CI
2.6 mm
3.2 mm
4.0 mm
For repairing of cracks, filling of defects and joining of all kind of
Cast Iron, Gray and Ductile Cast Iron.
Welding of dissimilar metals such as Cast Iron to all kind of steel
or stainless steel.
Shield Gas for DM-55M and DM-155M : 80% Ar + 20% CO2
N-100R
DM-55R
DM-155R
GTAW
Ar
1.6, 2.0, 2.4, 3.2 mm
x
1,000 mm
DM-55M
DM-155M
GMAW 1.2 / 1.6 mm
DM-30R Gas Welding 5.0 / 6.0 mm x 700mm
Product Name Welding Process Shield Gas Size (ø) Application
NICHIA 29-9 SMAW 2.6, 3.2,4.0 mm
Welding of dissimilar metals such as stainless steel to ferri
te steel or special steel like as SKD-11, SKD-61
Underlaying or build-up of Hard Surfacing
HE-500R GTAW Shield Gas :
Ar
1.6 ~ 3.2 mm
NFG-HE FCAW Shield Gas :
CO2
1.2 / 1.6 mm
LS-60
LS-80
SMAW 2.6, 3.2, 4.0 mm Welding of pressure vessels
600 ~ 800 Mpa Class High Tensile strength steel.
For heavy equipment industry, steel fabrication and Const
ruction equipments.
NTG-65SR
NTG-80SR
GTAW Shield Gas :
Ar
2.4 / 3.2 mm
NX-70
NX-80
GMAW Shield Gas :
80% Ar + 20
% CO2
1.2 / 1.6 mm
NICHIA-SMN SMAW 3.2 / 4.0 mm Joining of manganese steel and manganese steel
or dissimilar steel.
Joining of stainless steel and ferrite steel
NFG-SMN FCAW 1.2 / 1.6 mm
CAST IRON
DISSIMILAR – METAL OR SPECIAL METAL WELDING
NICHIA DM-100
Repairing Cast Iron
Welding for dissimilar metal S45C + SKD 61NICHIA 29-9
![Page 12: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/12.jpg)
6. Product Line up
Product Name Welding Process Hardness Size (ø) Application
NFG-HMN FCAW HRC 46-49 1.2 / 1.6 mm NFG-HMN Shield Gas : CO2
BK-700
BK-800K
NFG-H800S
SMAW
SMAW
FCAW
HRC 55~60
HRC 63~68
HRC 60~66
3.2, 4.0,
5.0 mm
1.2 / 1.6 mm
Hard surfacing of cutter knives, pump impellers, buckets, farm equipm
ent, forestry tools, and loading machines, etc
NFG-H800S Shield Gas : CO2
BKS-35CR
NFG-H30S
BK-30D
NFG-H30D
BK-30A
NFG-H30W
BK-1200
SMAW
FCAW
SMAW
FCAW
SMAW
FCAW
SMAW
HRC 56~61
HRC 57~62
HRC 62~66
HRC 61~65
HRC 63~68
HRC 63~68
Hv 1000
3.2~5.0 mm
1.2 / 1.6 mm
3.2~5.0 mm
1.2 / 1.6 mm
3.2~5.0 mm
1.6 mm
6.0 mm
For Heavy Soil abrasion and Erosive Abrasion
Hard Surfacing of Edge Runners, Chutes, Pump Casings,
Pump Impellers and Sand Blasts, Screw Conveyors.
Hard Surfacing of cutter knives, speed Muller, constructing machinery,
and mining machinery, etc.
Hard Surfacing of various parts which requested high temperature Abr
asion and Erosive Abrasion.
BK-1200 : Tubular type electrode
NFG-H30S, NFG-H30D, NFG-H30W (Shield Gas : CO2)
HARD SURFACING (Heavy equipment, facility )
Hard Surfacing of Molds BKH-61 Crushing Bucket Crushing Mill
NICHIA
![Page 13: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/13.jpg)
6. Product Line up
Product Name Welding Process Spec (AWS) Size (ø) Aplikasi
N-100
N-100R
N-100M
SMAW
GTAW
GMAW
ENi-1
ERNi-1
3.2~5.0 mm
1.6~3.2 mm
1.2 / 1.6 mm
For Pure Nickel. Nickel 200, 201.
Welding of Nickel & Nickel Alloys, dissimilar metals such as Ni
ckel to steel, Nickel to Stainless Steel.
NME
NME-R
NME-M
SMAW
GTAW
GMAW
ENiCu-7
ERNiCu-7
3.2~5.0 mm
1.6~3.2 mm
1.2 / 1.6 mm
For MONEL metal, MONEL Alloy 400.
Welding of MONEL & MONEL clad steel, lining welding of car
bon steel.
Joining dissimilar metal such as nickel and Cupro-Nickel.
NHC-2
NHC-2R
NHC-2M
SMAW
GTAW
GMAW
ENiCrMo-4
ERNiCrMo-4
3.2~5.0 mm
1.6~3.2 mm
1.2 /1.6 mm
For HASTELLOY C, C276
Welding of Hastelloy C, welding between Hastelloy C and diss
imilar metals, surfacing of valve seats, forging parts which cor
rosion resistibility is required.
NIN-182
NIN-82R
NIN-82M
NFG-82T
SMAW
GTAW
GMAW
FCAW
ENiCrFe-3
ERNiCr-3
ENiCr3T0-4
3.2~5.0 mm
1.6~3.2 mm
1.2 / 1.6 mm
1.2 /1.6 mm
For INCONEL 600, 601 and INCOLY 800, 800H
Welding of dissimilar metals such as Stainless Steel and INCO
NEL Alloys, carbon steels and INCONEL Alloys.
Build-up parts which heat or corrosion resistibility is required
.
NIN-625
NIN-625R
NIN-625M
NFG-625T
SMAW
GTAW
GMAW
FCAW
ENiCrMo-3
ERNiCrMo-3
ENiCrMo3T1-4
3.2~5.0 mm
1.6~4.0 mm
1.2 / 1.6 mm
1.2 / 1.6 mm
For INCONEL 625.
Welding of dissimilar metals such as INCONEL Alloys to stainl
ess steel, carbon steel.
Suitable for steels which heat or corrosion resistibility is requ
ired.
Nickel Tig Mig & Submerged Arc Welding Wire : Alloy W (ERNiMo-3), Alloy X (ERNiCrMo-2)
Alloy 59 (ERNiCrMo-13), Alloy 617 (ERNiCrCoMo-1)
Alloy 622 (ERNiCrMo-10), Alloy 718 (ERNiFeCr-2), Alloy 825 (ERNiFeCr-1)
NICKEL ALLOYS
Welding for Nickel 200 Welding for Hastelloy C276 Welding for HastelloyN-100R NHC-2R NHC-2
![Page 14: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/14.jpg)
6. Product Line up
Product Name Welding Process Spec (AWS) Size (ø) Application
NCU-D
NCU-R
NCU-M
SMAW
GTAW
GMAW
ECU
ERCu
3.2~5.0 mm
1.6~4.0 mm
0.9~1.6 mm
For Pure Copper.
Repair Welding of electrode holder, flange, and the parts which req
uired electric conductivity.
NCP
NCP-R
NCP-M
SMAW
GTAW
GMAW
ECuSn-C
ERCuSn-C
2.6~4.0 mm
1.2~4.0 mm
0.9~1.6 mm
For Phospher bronze.
Used for welding of Various kind of copper alloys such as phospher
bronze, brass and copper to brass.
NCS-R
NCS-M
GTAW
GMAW
ERCuSi-A 1.6~4.0 mm
1.2~1.6 mm
For Silicon Bronze.
Welding of similar and dissimilar metals of various copper alloys suc
h as pure copper, brass, gun metal and bronze.
NAC-8
NAC-10R
NAC-10M
SMAW
GTAW
GMAW
ECuAl-A2
ERCuAl-A2
3.2~4.0 mm
1.6~4.0 mm
0.9~1.6 mm
For Aluminum Bronze.
Welding of Aluminum Bronze.
Build-up parts which corrosion resistance is required.
NAB-5R
NAB-5M
GTAW
GMAW
ERCuAlNi 1.6~3.2 mm
0.8~1.6 mm
For Aluminum Nickel Bronze.
Welding of special Aluminum Bronze.
NCN-10D
NCN-10R
NCN-10M
NCN-30D
NCN-30R
NCN-30M
SMAW
GTAW
GMAW
SMAW
GTAW
GMAW
JIS D CuNi-1
JIS Y CuNi-1
ECuNi
ERCuNi
3.2~4.0 mm
1.6~4.0 mm
0.8~1.6 mm
3.2~5.0 mm
1.6~4.0 mm
0.8~1.6 mm
For cupro-nickel.
Welding of cupro-nickel and cupro-nickel clad steel.
Build-Up welding of carbon steel of similar and dissimilar metals of v
arious copper Alloys.
NICHIA TOHBIN Oxy-Acetylene flame
(Gas Welding)
2.0, 2.6
3.0 mm
Suitable to welding of similar metals and dissimilar metals such as c
opper alloys, general of copper brass, bronze to mild steel, special st
eel and Cast Iron.
COPPER & COPPER ALLOY
NICHIA
![Page 15: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/15.jpg)
6. Product Line up
Product Name Welding Process Spec (AWS) SIze (ø) Application
NS-4043 SMAW E4043 2.6~4.0 mm For arc welding aluminums alloyed with copper silicon and ma
gnesium, also excellent for joining dissimilar grades of Alumin
um.
A4043 WY
A4043 BY
A5356 WY
A5356 BY
A1100 WY
A1100 BY
A5183 WY
A5183 BY
A4047 WY
A4047 BY
GMAW
GTAW
GMAW
GTAW
GMAW
GTAW
GMAW
GTAW
GMAW
GTAW
ER 4043
R 4043
ER 5356
R 5356
ER 1100
R 1100
ER 5183
R 5183
ER4047
R4047
0.6, 0.8, 1.0,
1.2, 1.6, 2.0,
2.4 mm
(MIG)
1.2, 1.6, 2.0,
2.4, 3.2, 4.0,
5.0 mm
(TIG)
NIKKEI ALUMINUM WELDING WIRES
Welding of similar and dissimilar Aluminum materials.
For : AC7A, AC4D, A1070, A1050, A1100, A1200, A3004, A500
5, A5N01, A5052, A5652, A5154, A5354, A5086, A5083, A5056
, A6061, A6N01, A6063, A6101, A7003, A71N01 etc.
ALUMINUM WELDING MATERIALS
TITANIUM WELDING MATERIALSProduct Type Spec (AWS) Product Type Spec (AWS) Size(ø) Application
NTI-R
NTI-2R
NTI-3R
NTI-64R
NTI-7R
NTI-325R
NTI-12R
GTAW
ERTi-1
ERTi-2
ERTi-3
ERTi-5
ERTi-7
ERTi-9
ERTi-12
NTi-M
NTi-2M
NTi-3M
NTi-64M
NTi-7M
NTi-325M
NTi-12M
GMAW
ERTi-1
ERTi-2
ERTi-3
ERTi-5
ERTi-7
ERTi-9
ERTi-12
0.8, 0.9, 1.0,
1.2, 1.6, 2.0,
2.4, 3.2 mm
(GTAW)
0.8, 0.9, 1.0,
1.2, 1.6 mm
(GMAW)
For Titanium class 1 and class 2.
For Titanium class 1 and class 2.
For Titanium class 3.
For Titanium alloy (6%Al – 4%V – Ti)
For Titanium alloy containing Pd.
For Titanium alloy (3%Al – 2.5%V – Ti)
For Titanium alloy containing Ni.
Aluminum TIG Welding Titanium TIG Welding
NICHIA
![Page 16: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/16.jpg)
6. Product Line up
Product Name Spec (AWS) Size (ø) Application
BCup 2 <Harris 0>
BCup 3 <Stay-Silv5>
BCup 6
BCup 4
BCup 5 <Stay-Silv15>
BLOCKADE Bare
BLOCKADE FC
Silver 0%
Silver 5%
Silver 2%
Silver 6%
Silver 15%
(BCup – 9)
1.6, 2.0,
2.4, 3.2
mm
1. PHOSPHER COPPER
These brazing silver metals are primarily need to join copper
to copper, copper to brass, and brass to brass. These low coa
t alloys is suitable for most copper to copper or brass joints
where good fit up exists.
BAg-1
BAg-2
BAg-3
BAg-35 <Safety-Silv35>
BAg-36 <Safety-Silv45T>
LAg-37
LAg-45
Ag 41% Cd 25%
Ag 31% Cd 18%
Ag 50% Cd 16%
Ag 35% Zn 33%
Ag 45% + Zn + Tin
1.6, 2.0,
2.4, 3.2
mm
2. HIGH SILVER
General purpose Fiber for steel and copper, tungsten carbide
, stainless steel, nickel alloys make other steels, High Silver
metal alloys make premium quality braze.Ag 35% Flux Coated
Ag 45% Flux Coated
1.6 mm
ALSOLDER 500 (Harris)
T-235 (Almit)
1.6 / 3.2
mm
Soldering materials. Used to join all aluminum alloys to each
other and to dissimilar metals.
Product Name Application
Copper Flux For brazing welding flux, BCup 2, BCup 3, BCup 5.
STAY-SILV (White) Flux An all purpose, low temperature flux for use in silver brazing (570oC ~ 871oC)
STAY-SILV (Black) Flux High temperature flux for use in silver brazing, such as with stainless steel alloys, carbide,
heavy parts (570oC ~ 982oC).
TF-Flux
Stay-Clean Aluminum Flux
For use with aluminum soldering, works to join aluminum to dissimilar metals (Al + Al, Al +
Cu, Al +Fe).
Al-Braze EC Aluminum powdered Brazing Flux.
For use with aluminum brazing alloys such as Al1100, Al4047.
BRAZING & SOLDERING WELDING MATERIALS
FLUX FOR BRAZING & SOLDERING WELDING MATERIALS
![Page 17: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/17.jpg)
6. Product Line up
Product Name Size (ø) Application
TSW-420J2
TSW-308
TSW-316L
TSW-NC1
TSW-NA301
TSW-NHC276
1.6 mm,
3.17 mm (1/8”)
For corrosion, high temperature, abrasion & wear protecting.
For corrosion.
For corrosion.
For underlaying (buffer) & corrosion.
For corrosion, Hastelloy C.
For corrosion.
SN-Zinc 99.99
SN-Tin-Zinc
SN-Zinc-AL
SN-AL1070
SN-AL99999
1.0 mm
1.6 mm
3.17 mm(1/8”)
For steel structure to prevent from corrosion.
For film capaciter, corrosion.
For corrosion.
For corrosion film capaciter, vapor deposition for film capaciter.
For vapor deposition for packaging.
TSW-CuAL10
TSW-NCP3
TSW-NCUM
TSW-NCZM
1.6 mm
3.17 mm (1/8”)
For sliding wear resistance, piston & cylinder.
For corrosion or abrasion resistibility.
For electric conductivity corrosion.
For corrosion or abrasion resistibility.
We can supply Metal-Alloy powders, carbide powder & ceramics powder, etc.
THERMAL SPRAYING MATERIALS
Product Name Spec (AWS) Size (ø) Application
WT-20 (RED)
WL-15 (GOLD)
WL-20 (BLUE)
WC-20 (GRAY)
W-PURE (GREEN)
WZ-8 (WHITE)
Thorium 2.0%
Lanthan 1.5%
Lanthan 2.0%
Cerium 2.0%
Pure Tungsten
Zirconium0.8%
1.0, 1.2, 1.
6, 2.0,
2.4, 3.2,
4.0, 5.0,
6.0, 8.0, 10
.0 mm
X
150mm
Specialized NICHIA Tungsten Electrode will be your best choice for mai
ntaining your welding machine and improving the welding quality.
WT-20 For Steel, SUS, Ni, Cu, Alloys
WL-15 : For AC or DC
WC-20 : For low current, plastic molds
WZ-8 : For high load current
W-Pure : For AC
Tungsten ELECTRODE SHARPNER
TA-60XW
(AC 100V or 220V 50/60 HZ)
Simple operation : No skill required
Accurate Sharpening - Angle and Centering
Excellent Operability & Safety
TUNGSTEN ELECTRODE & SHARPENING MACHINE
![Page 18: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/18.jpg)
6. Product Line up
Portable Electrod Dry Oven ( YUNCHANG e-dryer)
Regulator
Electrode Capacity 7 Kg(11 lbs.)
Volts AC 220V
Hz 50Hz~60Hz
Watts 100W~200W
Temperature 50℃~250℃
Exterior Length 525 mm
Temp Control Adjustable Dial
MYUNGSHIN CO2 Regulator with heaterMYUNGSHIN Argon Regulator MYUNGSHIN OX/AC Regulator
![Page 19: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/19.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Silver Brazing
Silver Brazing flux
![Page 20: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/20.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Gouging
PVC Welding
![Page 21: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/21.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Welding machine
![Page 22: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/22.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Welding cable & Accessories
Superflex Welding cable Kurt Haufe Welding Holder, Cable connector, scun
Blue Eagle Welding mask, Glass Gosave Welding gloves, Plainsman TIG Gloves
![Page 23: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/23.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
TIG/MIG Torch & Accessories
Miller (Weld Craft) TIG Torch Miller (Weld Craft) TIG Torch Accessories
Binzel, Trafimet MIG Torch Binzel, Panasonic MIG Torch Accessories
![Page 24: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/24.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Grinding /Cutting / Drilling
Nippon Resibon Cutting DiscsMAKITA Tools ULTRA / WD Cutting Discs NORTON Grinding Discs
BOSH / HITACHI ToolsBench Drilling machines NACHI / YG-1 Cend Mills Tungsten Carbide Tips
![Page 25: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/25.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Gas, Gas Hose, Gas Cutting machine & torch
VICTOR, KOIKE, CHIYODA Gas Cutting Set KOIKE, YUKWANG Automatic gas Cutting machine
Gas hose coupler
Flash back arrestor
BRIDGESTONE, NCR, TOGAWA Gas Hose
![Page 26: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/26.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Power Equipment / loading tools
ENERPAC high pressure hydraulic toolsSUNRUN hydraulic jacks & tools
VITAL Block chainsHITACHIElectric chain hoist SPANSET webbing slings
![Page 27: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/27.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Hand tools
ELORA Hand tools TEKIRO / WIPRO Hand tools
Bolt & Nuts / Scaffoldings
Bolt & Nuts Scaffoldings
![Page 28: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/28.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Measurements/Guages
Vernier caliper
Digimatic caliper
Outside micrometer
Inside micrometer
Dial indicater
Digimatic indicater
Bore gauge
Interchangeable outsid micrometer
Welding gauge Thickness gauge Tape measure Digital Tester
Level scale Laser level Distance measuring wheel Digital scale KYOWA hydraulic pressure test pump
![Page 29: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/29.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Generator
Compressor
Air hose
Compressor 3 coupler
coupler Electric cable
![Page 30: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/30.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Valve
Bearings
KITZ Valve ONDA Valve
SKF Bearings NTN Bearings
![Page 31: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/31.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Fire fighting / Gas detector
Fans & HT
Shinwoo Gas detector
MOTOROLA HT set / RepeatersCKE industrial fans
![Page 32: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/32.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Chemicals, Lubricants
Paint / Brush / Spray Adhesives Anti-rust, coat, cleaners
Mega check / Magnaflux Crack detectionTemperature indicating crayons / Paint stick Sealant / caulking gun
3M Tapes
![Page 33: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/33.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
LED Lamp
Crosby shackles
Steel Plate / Wire rope
Kiswire Wire ropeKrakatau Steel plate / Rebar / H beam
TALLED Spot LED / Flood Lights
![Page 34: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/34.jpg)
6. Product Line up
Industrial tools and materials optimized in Indonesian local work environment and condition
Protective equipment
Safety Helmet Body harness Safety shoesSafety glasses
Safety gloves Safety mask / respirators / ear plugs
![Page 35: SeoulNikko€¦ · Company Name Seoul Nikko Co., Ltd Business Fields Welding Materials Welding Machines Welding Consumables Establishment 1995. 7 Address Seoul, Korea Contact +82](https://reader036.vdocuments.mx/reader036/viewer/2022062311/5ebc1c8df2ee8609d844cd8b/html5/thumbnails/35.jpg)
7. Why PT. Seoul Nikko Indonesia?
Strategic Price
One stop shopping service
for customer convenience
Stockiest for fast delivery
Technical support &
Global Network
Our Concern is
your convenience
& competitiveness