Page 2: Sample Review

SUB21261-02 (W-271AVB)The counter sink on the holes on the cover

panel(MPM20341)for the screw need to be widen. This is to ensure that the screw head sits flush with the panel and does

not stick out

Page 3: Sample Review

(W271AVB)IMPERFECTIONS IN THE POWDERCOATING.

Page 4: Sample Review

(W-343B)

1 out of 4 caster plates are welded in the wrong position.

This is the plate that is welded correctly.

Page 5: Sample Review

MPM50376-BR180 (W-343B)

BURN MARK ON THE BASE. CORNERS ON TOP SURFACE OF BASE ARE NOT POLISHED TO A CLEAN 45 DEGREES.

Page 6: Sample Review

MPM50377-BR180 (W-343B)

NOT EVENLY POLISHED. BURN MARK ON THE END CAP.

Page 7: Sample Review

MPM91183-09W (W-271VA)

VISIBLE GRIND MARKS THROUGH THE POWDER COATING. CAME IN WITH SCRATCHES .

Page 8: Sample Review

MPM20345-09W (W-271VA)

HOLE IS OBLONG AND CAUSES THE SCREW TO BE LOOSE INSIDE THE HOLE.

Page 9: Sample Review

MPM20314-09W (W-271VA)

THREADS ON THE WELD NUTS ARE 10MM AND VIRA DRAWING CALLS FOR THEM TO BE 3/8-16.

WELDNUTS WERE WELDED FLUSH WITH THE END OF THE TUBE AND SHOULD HAVE BEEN RECESSED 1/8” AS PER VIRA DRAWING.

Page 10: Sample Review

MPM10537-09W (W-271VA)

Flanges came in with wavy polishing on the top surface.

Page 11: Sample Review

MPM20324-09W (W-273VAB)

WAVY POLISHING ON TOP SURFACE WHERE BUSHINGS ARE TIG WELDED. OBLONG THRU HOLE.

Page 12: Sample Review

(W-273VAB)ID OF METAL SLEEVE WERE MEASURED AT .262”DIA. VIRA DRAWING CALLS IT TO BE .280”DIA HOLD.

PUCK FACE ON THE RIGHT IS OUR VENDOR’S QUALITY. PUCK FACE ON THE LEFT IS VIRA REWORK QUALITY.

Page 13: Sample Review

MPM02282-09W (W-350AV2)

1 WAS MADE THE CORRECT LENGTH OF 41 5/8”. THE OTHER ONE WAS MADE 44”L WHICH IS INCORRECT.

Page 14: Sample Review

MPM02283-09W (W-350AV2)

1 OUT OF 4 WAS MADE THE CORRECT LENGTH OF 43 5/8”. THE OTHER 3 WERE MADE 43 3/8”L.