Report copyright - HIGH CYCLE FATIGUE PROPERTIES OF AS-BUILT TI6AL4V (ELI ... · Ti6Al4V fatigue fracture surfaces [14, 15, 16]. All the fractographs showed areas of crack initiation, slow crack propagation,