Report copyright - STRESS CORROSION CRACKING STUDIES by …digitool.library.mcgill.ca/thesisfile112800.pdfSTRESS CORROSION CRACKING STUDIES IN CARTRIDGE BRASS by Charles D. Easteal A thesis submitted