Page 1: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

DAY 20: MORE ON METALS

Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion.

Page 2: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

TITANIUM

Light metal: 4.5 g/cm3 vs 7.9 g/cm3 for steel. Can be very strong: UTS up to 200 ksi.

Competitive with steel at a fraction of the weight, but you have to pay the price.

Very corrosion resistant. Forms a tenacious passive oxide layer on the surface.

Very reactive at high temperatures. Has to be produced in special process. Expensive.

3’ x 2’ x 3/16 in will cost about $1300. Titanium Overview (double click to access)

Page 3: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

MORE ON TITANIUM

Wikipedia says up to 77 tons will be used in each A-380.

Extremely corrosion resistant.

Now also seeing commodity use. Be careful, it might be a fake. I.e. golf clubs!

Komsomolets: Soviet era attack sub had Titanium hull.

OR DID IT?

Page 4: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

COPPER

Heavier than Fe, about 9.0 gm/cc. One of the earliest metals. MP 1100C. In unalloyed form, not very strong, but

extremely ductile. Yield: 5 Ksi, UTS: 30.5 Ksi, %EL = 60%.

Electical conductivity is key to its use in all kinds of electrical equipment and conductors.

Copper is also the base metal for two families of alloys:

1. Brasses (with Zn)2. Bronzes (with Sn and other metals)

Page 5: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

BRASS

Very attractive metal. Excellent corrosion resistance. Excellent ductility

Cartridge brass: 30%Zn

Yield 63 KsiUTS 76 KsiDuctility %EL = 8%

(After cold working.)

Page 6: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

BRONZE

Numerous alloys based on Sn, Ni, Aluminum, etc. Tin bronze: UTS is 45 ksi, Yield is 22 ksi, %EL =

25%. (Cast alloy) Used for bearings, bushings, fittings and gears.

Page 7: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

MAGNESIUM Very light metal. Density is about 1.7 gm/cm3.

HCP crystal structure. Elastic modulus and strength low. Some alloys may be precipitation hardened.

Get up to 50 ksi. Ductility somewhat limited. Around 10-15%. Clearly this metal has an excellent

strength/weight ratio – used in the aircraft industry.

Is also castable. Used as a substitue for plastic in casings for computers and other such stuff.

Corrosion resistance ok in normal environments, but quite poor in challenging environments.

Page 8: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

MAGNESIUM

http://www.asiagiken.co.jp/english/image/application07.jpg

http://photography-on-the.net/forum/showthread.php?t=57119 7

http://www.store.commoto.com/images/hypermotard-magnesium-clutc.jpg

Page 9: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

ZINC

Inexpensive Not strong, UTS about 5 Ksi. Not a strength

metal. MP about 420 C– Castable YES. Very good for

cheap commodity castings Very active metal! Used widely for plating

steel.

Page 10: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

ZINC USAGE

www.industrialmetalcasting.com/zinc-casting.html

http://alloydie.com/images/Zinc3.jpg

Page 11: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

http://minerals.usgs.gov/minerals/pubs/commodity/nickel/myb1-2006-nicke.pdf

NICKEL

Page 12: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

NICKEL

Most of all nickel produced goes into stainless steel

80% Ni/20% Cr alloys have been used as heating elements.

A major application of electroless nickel today is in computer hard discs

Rechargeable batteries can be nickel-cadmium or nickel metal

http://www.nickelinstitute.org/index.cfm/ci_id/16/la_id/1.htmhydride

Page 13: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

SUPERALLOYS

These alloys are intended to be as strong as possible at high temperatures.

The base metal is Fe, Co, or Ni. The latter is most often used in aircraft engines.

The most common solutes are Al and Ti. Result is two main phases: and ’.Actually, many different metals are added as solutes to achieve various strengthening effects.

It is possible to get a turbine blade which is a single crystal, later to be strengthened with the precipitation of the second phase.

Page 14: D AY 20: M ORE ON M ETALS Titanium Copper Magnesium Zinc Nickel Superalloys Material selection discussion

MATERIALS SELECTION

Brief Example Each group will try to pick a number of

candidate materials that meet the requirements of each device.

Some groups will be selected to make reports.