Supplementary material: Influence of TiO 2 agglomerate and aggregate sizes on photocatalytic activity Figure 1: Measured spectra in the range of 600 - 300 nm of the used light source (Philips 40W UEO Performance) for the photocatalytic experiments. Light intensities were measured separately for every reactor.

Upload: truongnhan

Post on 09-Mar-2018

213 views

Category:

Documents


0 download

TRANSCRIPT

Page 1: 10853_2016_400_MOESM1_ESM.docx - Springer …10.1007... · Web viewFormation of HCHO in the presence of the diluted (left) and freeze dried (right) catalyst suspension (1 g L-1) out

Supplementary material: Influence of TiO2 agglomerate and aggregate sizes on photocatalytic activity

Figure 1: Measured spectra in the range of 600 - 300 nm of the used light source (Philips 40W UEO Performance) for the photocatalytic experiments. Light intensities were measured separately for every reactor.

Page 2: 10853_2016_400_MOESM1_ESM.docx - Springer …10.1007... · Web viewFormation of HCHO in the presence of the diluted (left) and freeze dried (right) catalyst suspension (1 g L-1) out

Figure 2: Formation of HCHO in the presence of the diluted (left) and freeze dried (right) catalyst suspension (1 g L-1) out of a 30 mM MeOH solution. Illuminatiuon was performed with a Philips 40W UEO Performance lamp.

Page 3: 10853_2016_400_MOESM1_ESM.docx - Springer …10.1007... · Web viewFormation of HCHO in the presence of the diluted (left) and freeze dried (right) catalyst suspension (1 g L-1) out

Figure 3: TEM images of freeze dried suspensions. 0.5 h (top, left), 4 h (top right),

96 h (bottom, left), XXS100 (bottom right).

Figure 4: Rheological properties of the used suspensions.

Figure 5: Agglomerated particle size distribution of the used suspensions measured with DLS.